Shandong, China
Business Type:
Number of Employees:
Year of Establishment:
Management System Certification:
OEM/ODM Service
Sample Available

Aluminum Welding Wire, Welding Wire, Welding Material manufacturer / supplier in China, offering Factory Aluminum Welding Wire Er4043 with CCS, ABS, Dnv, 5.0mm 500kg Packing Em12K Submerged Arc Welding Wire with Ce Certificate, Er70s-6 Welding Wire with Ce CCS ISO and so on.

Gold Member Since 2014
Audited Supplier
Supplier Homepage Products Aluminium Welding Wire Factory Aluminum Welding Wire Er4043 with CCS, ABS, Dnv

Factory Aluminum Welding Wire Er4043 with CCS, ABS, Dnv

Get Latest Price
Purchase Qty. / Reference FOB Price
1-4 Tons US $5,400
5+ Tons US $5,350
Port: Tianjin, China
Production Capacity: 2000 Tons Per Year
Payment Terms: L/C, T/T, D/P
Type: Rolling Wire
Material: Aluminum / Aluminum Alloy
Flux Containing: Not Containing Flux
Size: 1.6mm-4.0mm
Weight: 5kg,10kg
Raw Material: Aluminum

You Might Also Like


Basic Info

Model NO.: AWS ER4043
Packing: Carton,Pallet
Trademark: LUHAN
Transport Package: as Your Request
Specification: 1.6mm-4.0mm
Origin: China
HS Code: 76052900

Product Description

ER4043 is a kind of aluminium & silicon alloy welding wires with 5% silicon, also name S331, and this product is of good liquidity, good forgeability, but lack of ductility. Due to the high silicon content, when used in the welding of high magnesium alloy, easily generated in the weld brittle Mg2Si, reduce the plasticity and the corrosion resistance of joint. In addition, the welding surface color dark, anodized after more different with parent metal color.
Factory Aluminum Welding Wire Er4043 with CCS, ABS, Dnv
The argon arc welding of Aluminium alloy casting and workpiece is used as the filler material, special for 6061 and 6XXX series aluminium alloy, and 3XXX & 2XXX series aluminiumalloy welding, widely used in ships, engine, chemistry, food, sports, uipment, mould, furniture, vessel, container, etc.
ER4043 aluminium & silicon is with high of crack resistance, but low plasticity, so for Plastic deformation joints after welding, we donor suggest it. You should strictly clean the oxide film on the edge of the workpiece and oil before welding, otherwise it will make bad weld produce and cause porosity, slag inclusion and other defects. Also you can use a plate to hold molten metal to ensure meld form.
Wire Standard
ANSI/AWS A5.10-92
Passed ISO9001: 2008 Quality Management System
Chemical component(wt)/%
OthersOthers total
Melting range1065 - 1170°F
Electrical conductivity42%IACS(O)
Anti corrosion performanceB(Gen) A(SCC)
The coefficient of thermal expansion (20  ~300)22×10-6/K
Thermal conductivity (20 )170W/m@K