Production Capacity: 30000 Tons Per Year
Payment Terms: L/C, T/T, D/P

Request a custom order and have something just for you!

Send Customized Request
Basic Info
  • Model NO.: AWS A5.10
  • Material: Aluminum / Aluminum Alloy
  • Diameter: 0.8\0.9\1.0\1.2\1.6
  • Transport Package: as Your Request
  • Origin: Shandong, China
  • Type: Rolling Wire
  • Flux Containing: Not Containing Flux
  • Trademark: Luhan/Tianlei
  • Specification: 0.8-1.6mm
  • HS Code: 72292000
Product Description
Packaging & Delivery

Packaging Details:
0.50kg/spool or 1lb/spool 1.0kg/spool or 2lb/spool 2.0kg/spool or 5lb/spool 5.0kg/spool or 12lb/spool 7.0kg/spool or 16lb/spool Standrad strong export packing or as per customer ordered
Delivery Detail:Within 15 days after order comfirmation

Specifications
1. Low welding costs. 
2. High productivity and low electricity consumption. 
3. Easy to operate.
Technology data for your reference:

AWS

Joint Strength

 Parent metal

Characteristics

Standard

(Mpa)

ER1070

Above 55

Pure aluminum series105010701080

Good anti-corrosive and plasticity

ER1100

80-110

Pure aluminum  series1100

Good anti-corrosive and plasticity

ER1200

80-110

Pure aluminum  series1200

Good anti-corrosive and plasticity

ER2319

400-450

Pure aluminum  series2219

High intensity after heat treatment

ER4043

170-250

Al-Mg-Si casting aluminum

The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process

ER4047

170-250

Casting Al. ,Al-Cu casting ,Ag-Mg-Si casting

The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process

ER4145

200-300

Al-Cucasting20142017

The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process

ER5554

180-240

low Mg content5052,5454casting

 Use chemical equipment with a temperature above 65

ER5654

210-270

medium Mg content5154casting

medium intensity,good anti-corrosive

ER5356

270-310

Al-Mg casting, Al-Mg-Si casting, Al-Zn-Mg casting

Typical welding wire used most widely, good mechanics performance and anti-corrosiveness

ER5556

280-320

Al-Zn-Mg casting, Al-Mg casting

The connector intensity is high, and the moulding performance and tenacity is inferior to 5183

ER5183

280-310

Al-Mgcasting5083

Typical welding wire used most widely, good mechanical performance and anti-corrosiveness

Aluminum Welding Wire Er1100 (AWS A5.10)
Send your message to this supplier
Avatar
Mrs. Melody
Business Manager
*From:
To: Mrs. Melody
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now